REFLECTOR: humidity and baffle thickness

John Tvedte johnt at comp-sol.com
Wed Apr 9 14:42:15 CDT 2008


Pretty sure I remember reading that humidity is required for Jeffco to cure....

Of course, I'm not 100% sure - so - I'd either call the factory, or call a support Engr. at Jeffco.

John

________________________________________
From: reflector-bounces at tvbf.org [reflector-bounces at tvbf.org] On Behalf Of doug.holub at tx.rr.com [doug.holub at tx.rr.com]
Sent: Wednesday, April 09, 2008 9:55 AM
To: reflector at tvbf.org
Subject: REFLECTOR: humidity and baffle thickness

I'm re-sealing my fuel tanks this week and I'm a little paranoid. It's raining in Dallas today. Is there any problem using Jeffco (or EZ-Poxy) when the humidity is high?

On another subject, I think I'm just going to make aluminum engine baffles instead of using the factory's plenum and runners. Can anyone recommend a material thickness? I'm thinking around .020 or .025.

Doug Holub
Standard FG 90% done, 20% to go
_______________________________________________
To change your email address, visit http://www.tvbf.org/mailman/listinfo/reflector

Visit the gallery!  www.tvbf.org/gallery
user:pw = tvbf:jamaicangoose
Check new archives: www.tvbf.org/pipermail
Check old archives: http://www.tvbf.org/archives/velocity/maillist.html



More information about the Reflector mailing list